产品名称 | 编号 | 规格 | 包装 |
---|---|---|---|
BeaverBeads™ Mag COOH | 70106-5 | 300nm 10mg/mL | 5mL |
BeaverBeads™ Mag COOH | 70106-50 | 300nm 10mg/mL | 50mL |
BeaverBeads™ Mag COOH | 70107-5 | 10mg/mL,500nm | 5mL |
BeaverBeads™ Mag COOH | 70107-50 | 10mg/mL,500nm | 50mL |
BeaverBeads™ Mag COOH | 70104-5 | 1μm 10mg/mL | 5mL |
BeaverBeads™ Mag COOH | 70104-50 | 1μm 10mg/mL | 50mL |
BeaverBeads™ Mag COOH | 70102-5 | 2μm 10mg/mL | 5mL |
BeaverBeads™ Mag COOH | 70102-50 | 2μm 10mg/mL | 50mL |
BeaverBeads™ Mag COOH | 70105-5 | 5μm 10mg/mL | 5mL |
BeaverBeads™ Mag COOH | 70105-50 | 5μm 10mg/mL | 50mL |
BeaverBeads™ Magrose COOH | 70103-5 | 20%(v/v) | 5mL |
BeaverBeads™ Magrose COOH | 70103-50 | 20%(v/v) | 50mL |
BeaverBeads Mag COOH-NS500 | 70108-5 | 10 mg/mL,500nm | 5mL |
BeaverBeads Mag COOH-NS500 | 70108-50 | 10mg/mL,500nm | 50 mL |
产品名称 | Mag COOH | Magrose COOH |
粒径 | 30-150μm | |
表面基团/含量 | ~200μmol/g | ~50μmol/ml |
磁核 | Fe3O4 | Fe3O4 |
壳层 | 聚合物 | 琼脂糖 |
饱和磁化强度 | 40~60 emu/g | 30~50 emu/g |
应用方向 | 适用于诊断、检测 | 适用于分离、纯化 |
共同特点 | 超顺磁性,可自动/手动操作 | |
*水化平均粒径,Malvern Nano测定 |
Mag COOH产品特性 1. 羧基含量丰富:>100μmol/g; 2. 操作性能好:磁珠分散均匀,具有超顺磁性,磁响应时间<30s; 3. 稳定性及批次间重复性好:粒径均一,多分散系数<0.2,呈单分散;
| Magrose在倒置显微镜下400倍成像 |
---|---|
Magrose COOH偶联荧光多肽后在显微镜下成像 | Magrose COOH产品特性 1.羧基含量丰富:~1000μmol/g; 2. 操作性能好:磁珠分散均匀,具有超顺磁性,磁响应时间<10s; 3.稳定性及批次间重复性好,批间羧基含量CV<5%; 4.目标物质结合量高,非特异性吸附低:专用于分离、纯化领域。
|
应用方向 • 蛋白纯化 • 免疫检测 • 细胞分选 • 特异性核酸分离 • 生物传感器 • 药物筛选和输送 |
引用文献:
- A Rapid Detection Method of Brucella with Quantum Dots and Magnetic Beads Conjugated with Different Polyclonal Antibodies;Song et al. Nanoscale Research Letters (2017) 12:179,DOI:10.1186/s11671-017-1941-z